Update on the stress corrosion phenomenon and adjustment of 2022 French nuclear output estimate

Update on the stress corrosion phenomenon and adjustment of 2022 French nuclear output estimate

EDF is continuing its inspection programme and is preparing, along with the nuclear industry, to repair sections of the pipes affected by stress corrosion. At this stage for 2022, EDF considers that it is not necessary to schedule new reactor outages and updates its French nuclear output estimate.

Twelve reactors, currently shut down, are being inspected for stress corrosion:

  • Result of the metallurgical expertises carried out on samples taken from the pipes of the auxiliary circuits of the reactors of Civaux 1, Chooz 1 and Penly 1 confirmed the presence of stress corrosion near welds of the RIS (safety injection circuit) and RRA (shutdown reactor cooling circuit) circuits.
  • Checks and expertises carried out on Chinon B3 confirm the absence of stress corrosion on the SIS circuit. Evidence of stress corrosion was located on a weld of the RRA circuit.
  • Checks and investigations are ongoing on the other eight prioritized reactors (Civaux 2, Chooz 2, Cattenom 3, Bugey 3, Bugey 4, Flamanville 1, Flamanville 2 and Golfech 1).

EDF carried out ultrasonic inspections, investigations on pipes samples, digital welding simulations and studies to calculate the speed of propagation of stress corrosion.
At this stage, these analyses allow EDF to confirm slow stress-corrosion propagation and to observe the existence of a compression zone which blocks the propagation of the phenomenon.

EDF has defined an inspection programme for the entire nuclear fleet:

  • In 2022, 900MW reactors will be inspected as part of their ten-year inspection visits. This concerns Tricastin 3, Gravelines 3, Dampierre 2, Blayais 1, and Saint-Laurent B2 reactors.
  • The inspection programme for the 1,300MW reactors will be established after integrating the lessons learned from the appraisals and checks in progress on the auxiliary circuits of the Penly 1 reactor.

At this stage for 2022, EDF considers that new reactor outages do not need to be scheduled to carry out checks.
Discussions are ongoing with the Autorité de sûreté nucléaire (French Nuclear Safety Authority) on the stress corrosion phenomenon inspection and repair programme.

The nuclear industry is making an unprecedented, concerted effort to replace the portions of the pipes affected by stress corrosion.
EDF has started to procure tubes and elbows from European steelmakers. Production rates have been optimised to deliver the first spare parts before summer.
All of the qualified suppliers to carry out these activities are now preparing for the work. Dozens of welders have been specially trained to guarantee high-quality workmanship.

In view of all of these aspects and EDF’s decision to shut down impacted reactors and inspect the reactors likely to be impacted, ASN took note of EDF’s actions.

All of these events require EDF to adjust its French nuclear output estimate for 2022 to 280-300TWh against 295-315TWh previously.

At this stage and in the expectation of checks and repairs to be completed, the 2023 French nuclear output estimate is not changed (300-330TWh).

For illustrative purposes, based on the information available to the Group at this stage and on the 2022 forward prices on 18 May 2022, the estimate of the impact of the decrease in output on the Group’s EBITDA for 2022 is reassessed at approximately -€18,5 billion1.

Based on these same facts, the end of 2023 EDF group’s financial perspective is adjusted as follows: net financial debt/EBITDA ~3x or slightly higher than 3x, and adjusted net debt/adjusted EBITDA to ~5x 2,3.

This press release is certified. Check its authenticity on medias.edf.com

About d’EDF
As a major player in energy transition, the EDF Group is an integrated energy company active in all businesses: generation, transmission, distribution, energy trading, energy sales and energy services. EDF group is a world leader in low-carbon energy, having developed a diverse production mix based mainly on nuclear and renewable energy (including hydropower). It is also investing in new technologies to support energy transition. EDF’s raison d’être is to build a net zero energy future with electricity and innovative solutions and services, to help save the planet and drive well-being and economic development. The Group is involved in supplying energy and services to approximately 38.5 million customers (1), of whom 29.3 million in France (2). It generated consolidated sales of €84.5 billion in 2021. EDF is listed on the Paris Stock Exchange.

(1) Since 2018, customers are counted per delivery site. A customer can have two delivery points: one for electricity and another one for gas.
(2) Including ÉS (Électricité de Strasbourg) and SEI.


1 Versus 14 billion euros (see financial communication Q1 2022 – May 4, 2022)

2 Versus net financial debt/EBITDA ~3x and adjusted net debt/adjusted EBITDA 4.5x to 5x (at constant S&P methodology), see PR of May 4, 2022
3 Based on electricity prices for 2023 delivery on May 18, 2022 and excluding additional regulatory measures

Attachment

Disclaimer & Cookie Notice

Welcome to GOLDEA services for Professionals

Before you continue, please confirm the following:

Professional advisers only

I am a professional adviser and would like to visit the GOLDEA CAPITAL for Professionals website.

Important Notice for Investors:

The services and products offered by Goldalea Capital Ltd. are intended exclusively for professional market participants as defined by applicable laws and regulations. This typically includes institutional investors, qualified investors, and high-net-worth individuals who have sufficient knowledge, experience, resources, and independence to assess the risks of trading on their own.

No Investment Advice:

The information, analyses, and market data provided are for general information purposes only and do not constitute individual investment advice. They should not be construed as a basis for investment decisions and do not take into account the specific investment objectives, financial situation, or individual needs of any recipient.

High Risks:

Trading in financial instruments is associated with significant risks and may result in the complete loss of the invested capital. Goldalea Capital Ltd. accepts no liability for losses incurred as a result of the use of the information provided or the execution of transactions.

Sole Responsibility:

The decision to invest or not to invest is solely the responsibility of the investor. Investors should obtain comprehensive information about the risks involved before making any investment decision and, if necessary, seek independent advice.

No Guarantees:

Goldalea Capital Ltd. makes no warranties or representations as to the accuracy, completeness, or timeliness of the information provided. Markets are subject to constant change, and past performance is not a reliable indicator of future results.

Regional Restrictions:

The services offered by Goldalea Capital Ltd. may not be available to all persons or in all countries. It is the responsibility of the investor to ensure that they are authorized to use the services offered.

Please note: This disclaimer is for general information purposes only and does not replace individual legal or tax advice.